QUANTITATIVE COMPARISON OF PERMEABILITY IN THE ADHESIVE INTERFACE OF FOUR ADHESIVE SYSTEMS = 열순환 후 상아질 접착 계면의 수분 투과성 변화에 대한 정량적 분석
저자
장주혜 (Department of Conservative Dentistry and Dental Research Institute, School of Dentistry, Seoul National University) ; 이기욱 (Geochronology Team, Korea Basic Science Institute) ; 김혜영 (Craniomaxillofacial Life Science(BK 21), School of Dentistry, Seoul National University) ; 이인복 (Department of Conservative Dentistry and Dental Research Institute, School of Dentistry, Seoul National University) ; 조병훈 (Department of Conservative Dentistry and Dental Research Institute, School of Dentistry, Seoul National University) ; 손호현 (Department of Conservative Dentistry and Dental Research Institute, School of Dentistry, Seoul National University)
발행기관
학술지명
Restorative Dentistry & Endodontics(The Journal of Korean Academy of Conservative Dentistry)
권호사항
발행연도
2009
작성언어
English
주제어
KDC
510
등재정보
KCI등재
자료형태
학술저널
발행기관 URL
수록면
51-60(10쪽)
KCI 피인용횟수
1
제공처
본 연구는 현재 시판 되고 있는 여러 개의 상아질 접착제를 임상 술식에서와 같은 방법으로 사용한 다음 열순환 후 접착계면의 변화를 관찰 비교하고자 했다.
발거 한 지 한 달 이내인 대구치 28개의 교합 면 상아질 표면에 4종의 상아질 접착제 (OptiBond FL [OP], AdheSE [AD], Clearfil SE Bond [CL], Xeno Ⅲ [KE] 중 하나를 적용한 뒤 복합 레진 (Premisa, Kerr)을 1mm두께로 올린 후 광중합 하였다. 4℃ 증류수에서 6일간 보관한 뒤 치아의 정중선으로부터 수직으로 절단하여 그 중 절반의 치아에서 2mm 두께의 시편을 얻은 다음 남은 반쪽의 치아는 10.000회의 열순환을 가한 뒤 (5˚-55˚, 침지 시간 25초 대기 시간 5초) 같은 방법으로 2 mm 두께의 시편을 얻었다. 연마한 시편을 24시간 동안 50% ammoniacal silver nitrate solution에 담근 다응 photo-developing solution에서 8시간 동안 환원시켰다. 계면을 가로지르는 5개의 line 상에서 wavelength dispersive spectrometry (WDS) detector를 이용하여 주사선상에 있는 원소들의 중량비를 계산하였다 또한 열순환 전과 후의 시편에서 얻어진 5개의 silver 측정치를 서로 비교하였다.
열순환 전의 접착제층(adhesive layer)에서는 OP에서 가장 적은 silver의 투과가 관찰되었으며 (P<0.0001), CL. AD, XE 순으로 투과 량이 중가함을 보였다. 혼성층 (Hybrid layer) 에서는 CL의 투과량이 가장 적었다 (p=0.0039) 열순환 후에 접착제층과 혼성층에서 silver의 투과량은 증가하지는 않았다. Scanning electron microscopy(SEM) 사진을 통하여 각 시편의 접착 계면에서 접착제에 따른 특이적인 silver의 투과상을 관찰할 수 있었다. 전반적으로 OP와 CL의 접착계면이 열순환 과정 중에도 온전히 유지됨을 볼 수 있었다.
접착 계면에서의 수분 투과 양상은 각 접착제예 따라 다른 형태를 보였으며 열 순환에 의해 유의할 만한 변화를 야기하지는 않았다.
The purpose of this study was to perform quantitative comparisons of water permeable zones in both the adhesive and the hybrid layer before and after thermocycling in order to assess the integrity of the bonding interface. Twenty eight flat dentin surfaces were bonded with a light-cured composite resin using one of four commercial adhesives [OptiBond FL (OP), AdheSE (AD), Clearfil SE Bond (CL), and Xeno Ⅲ (XE)]. These were sectioned into halves and subsequently cut to yield 2-mm thick specimens: one specimen for control and the other subjected to thermocycling for 10,000 cycles. After specimens were immersed in ammoniacal silver nitrate for 24 h and exposed to a photo developing solution for 8 h. the bonded interface was analyzed by scanning election microscopy (SEM) and wavelength dispersive spectrometry (WDS) at five locations per specimen Immediately after bonding thc adhesive layer of OP showed the lowest silver uptake followed by CL, AD, and XE in ascending order (p< 0.0001) the hybrid layer of CL had the lowest silver content among the groups (p=0.0039) After thermocycling none of the adhesives manifested a significant increase of silver in either the adhesive or the hybrid layer. SEM demonstrated the characteristic silver penetrated patterns within the interface. It was observed that integrity of bonding was well maintained in OP and CL throughout the thermocycling process. Adhesive-tooth interfaces are vulnrable to hydrolytic degradation and its permeability varies in different adhesive systems, which may be clinically related to the restoration longevity.
더보기분석정보
연월일 | 이력구분 | 이력상세 | 등재구분 |
---|---|---|---|
2027 | 평가예정 | 재인증평가 신청대상 (재인증) | |
2021-01-01 | 평가 | 등재학술지 유지 (재인증) | KCI등재 |
2018-01-01 | 평가 | 등재학술지 선정 (계속평가) | KCI등재 |
2017-12-01 | 평가 | 등재후보로 하락 (계속평가) | KCI후보 |
2013-01-01 | 평가 | 등재 1차 FAIL (등재유지) | KCI등재 |
2010-01-01 | 평가 | 등재학술지 유지 (등재유지) | KCI등재 |
2008-01-01 | 평가 | 등재학술지 유지 (등재유지) | KCI등재 |
2005-01-01 | 평가 | 등재학술지 선정 (등재후보2차) | KCI등재 |
2004-01-01 | 평가 | 등재후보 1차 PASS (등재후보1차) | KCI후보 |
2003-01-01 | 평가 | 등재후보학술지 유지 (등재후보1차) | KCI후보 |
2002-01-01 | 평가 | 등재후보학술지 유지 (등재후보1차) | KCI후보 |
2000-07-01 | 평가 | 등재후보학술지 선정 (신규평가) | KCI후보 |
기준연도 | WOS-KCI 통합IF(2년) | KCIF(2년) | KCIF(3년) |
---|---|---|---|
2016 | 0.25 | 0.25 | 0.21 |
KCIF(4년) | KCIF(5년) | 중심성지수(3년) | 즉시성지수 |
0.21 | 0.19 | 0.448 | 0.1 |
서지정보 내보내기(Export)
닫기소장기관 정보
닫기권호소장정보
닫기오류접수
닫기오류 접수 확인
닫기음성서비스 신청
닫기음성서비스 신청 확인
닫기이용약관
닫기학술연구정보서비스 이용약관 (2017년 1월 1일 ~ 현재 적용)
학술연구정보서비스(이하 RISS)는 정보주체의 자유와 권리 보호를 위해 「개인정보 보호법」 및 관계 법령이 정한 바를 준수하여, 적법하게 개인정보를 처리하고 안전하게 관리하고 있습니다. 이에 「개인정보 보호법」 제30조에 따라 정보주체에게 개인정보 처리에 관한 절차 및 기준을 안내하고, 이와 관련한 고충을 신속하고 원활하게 처리할 수 있도록 하기 위하여 다음과 같이 개인정보 처리방침을 수립·공개합니다.
주요 개인정보 처리 표시(라벨링)
목 차
3년
또는 회원탈퇴시까지5년
(「전자상거래 등에서의 소비자보호에 관한3년
(「전자상거래 등에서의 소비자보호에 관한2년
이상(개인정보보호위원회 : 개인정보의 안전성 확보조치 기준)개인정보파일의 명칭 | 운영근거 / 처리목적 | 개인정보파일에 기록되는 개인정보의 항목 | 보유기간 | |
---|---|---|---|---|
학술연구정보서비스 이용자 가입정보 파일 | 한국교육학술정보원법 | 필수 | ID, 비밀번호, 성명, 생년월일, 신분(직업구분), 이메일, 소속분야, 웹진메일 수신동의 여부 | 3년 또는 탈퇴시 |
선택 | 소속기관명, 소속도서관명, 학과/부서명, 학번/직원번호, 휴대전화, 주소 |
구분 | 담당자 | 연락처 |
---|---|---|
KERIS 개인정보 보호책임자 | 정보보호본부 김태우 | - 이메일 : lsy@keris.or.kr - 전화번호 : 053-714-0439 - 팩스번호 : 053-714-0195 |
KERIS 개인정보 보호담당자 | 개인정보보호부 이상엽 | |
RISS 개인정보 보호책임자 | 대학학술본부 장금연 | - 이메일 : giltizen@keris.or.kr - 전화번호 : 053-714-0149 - 팩스번호 : 053-714-0194 |
RISS 개인정보 보호담당자 | 학술진흥부 길원진 |
자동로그아웃 안내
닫기인증오류 안내
닫기귀하께서는 휴면계정 전환 후 1년동안 회원정보 수집 및 이용에 대한
재동의를 하지 않으신 관계로 개인정보가 삭제되었습니다.
(참조 : RISS 이용약관 및 개인정보처리방침)
신규회원으로 가입하여 이용 부탁 드리며, 추가 문의는 고객센터로 연락 바랍니다.
- 기존 아이디 재사용 불가
휴면계정 안내
RISS는 [표준개인정보 보호지침]에 따라 2년을 주기로 개인정보 수집·이용에 관하여 (재)동의를 받고 있으며, (재)동의를 하지 않을 경우, 휴면계정으로 전환됩니다.
(※ 휴면계정은 원문이용 및 복사/대출 서비스를 이용할 수 없습니다.)
휴면계정으로 전환된 후 1년간 회원정보 수집·이용에 대한 재동의를 하지 않을 경우, RISS에서 자동탈퇴 및 개인정보가 삭제처리 됩니다.
고객센터 1599-3122
ARS번호+1번(회원가입 및 정보수정)