KCI등재후보
지혈제 오염이 콤포머의 전단결합강도에 미치는 영향 = THE EFFECTS OF SURFACE CONTAMINATION BY HEMOSTATIC AGENTS ON THE SHEAR BOND STRENGTH OF COMPOMER
One of this latest concepts in bonding are "total etch", in which both enamel and dentin are etched with an acid to remove the smear layers, and "wet dentin" in which the dentin is not dry but left moist before application of the bonding primer. Ideally, the application of a bonding agent to tooth structure should be insensitive to minor contamination from oral fluids. Clinically, contaminations such as saliva, gingival fluid, blood and handpiece lubricant are often encountered by dentists during cavity preparation.
The aim of this study was to evaluate the effect of contamination by hemostatic agents on shear bond strength of compomer restorations. One hundred and ten extracted human maxillary and mandibular molar teeth were collected. The teeth were removed soft tissue remnant and debris and stored in physiologic solution until they were used. Small flat area on dentin of the buccal surface were wet ground serially with 400, 800 and 1200 abrasive papers on automatic polishing machine. The teeth were randomly divided into 11 groups.
Each group was conditioned as follows:
Group 1: Dentin surface was not etched and not contaminated by hemostatic agents.
Group 2: Dentin surface was not etched but was contaminated by Astringedent® (Ultradent product Inc., Utah, U.S.A.).
Group 3: Dentin surface was not etched but was contaminated by Bosmin®(Jeil Pharm, Korea).).
Group 4: Dentin surface was not etched but was contaminated by Epri-dent®(Epr Industries, NJ, U.S.A.).
Group 5: Dentin surface was etched and not contaminated by hemostatic agents.
Group 6: Dentin surface was etched had contaminated by Astringedent®.
Group 7: Dentin surface was etched and contaminated by Bosmin®.
Group 8: Dentin surface was etched and contaminated by Epri-dent®.
Group 9: Dentin surface was contaminated by Astringedent®. The contaminated surface was rinsed by water and dried by compressed air.
Group 10: Dentin surface was contaminated by Bosmin®. The contaminated surface was rinsed by water and dried by compressed air.
Group 11: Dentin surface was contaminated by Epri-dent®. The contaminated surface was rinsed by water and dried by compressed air.
After surface conditioning. F2000® was applicated on the conditoned dentin surface.
The teeth thermocycled in distilled water at 5℃ and 55℃ for 1,000 cycles. The samples were placed on the binder with the bonded compomer-dentin interface paralled to the knife-edge shearing rod of the Universal Testing Machine(Zwick Z020, Zwick Co.,
Germany) running at a cross head speed of 1.0mm/min.
Group 2 showed significant decrease in shear bond strength compared with group 1 and group 6 showed significant decrease in shear bond strength compared with group 5.
There were no significant differences in shear bond strength between group 5 and group 9, 10 and 11.
분석정보
연월일 | 이력구분 | 이력상세 | 등재구분 |
---|---|---|---|
2027 | 평가예정 | 재인증평가 신청대상 (재인증) | |
2021-01-01 | 평가 | 등재학술지 유지 (재인증) | KCI등재 |
2018-01-01 | 평가 | 등재학술지 선정 (계속평가) | KCI등재 |
2017-12-01 | 평가 | 등재후보로 하락 (계속평가) | KCI후보 |
2013-01-01 | 평가 | 등재 1차 FAIL (등재유지) | KCI등재 |
2010-01-01 | 평가 | 등재학술지 유지 (등재유지) | KCI등재 |
2008-01-01 | 평가 | 등재학술지 유지 (등재유지) | KCI등재 |
2005-01-01 | 평가 | 등재학술지 선정 (등재후보2차) | KCI등재 |
2004-01-01 | 평가 | 등재후보 1차 PASS (등재후보1차) | KCI후보 |
2003-01-01 | 평가 | 등재후보학술지 유지 (등재후보1차) | KCI후보 |
2002-01-01 | 평가 | 등재후보학술지 유지 (등재후보1차) | KCI후보 |
2000-07-01 | 평가 | 등재후보학술지 선정 (신규평가) | KCI후보 |
기준연도 | WOS-KCI 통합IF(2년) | KCIF(2년) | KCIF(3년) |
---|---|---|---|
2016 | 0.25 | 0.25 | 0.21 |
KCIF(4년) | KCIF(5년) | 중심성지수(3년) | 즉시성지수 |
0.21 | 0.19 | 0.448 | 0.1 |
서지정보 내보내기(Export)
닫기소장기관 정보
닫기권호소장정보
닫기오류접수
닫기오류 접수 확인
닫기음성서비스 신청
닫기음성서비스 신청 확인
닫기이용약관
닫기학술연구정보서비스 이용약관 (2017년 1월 1일 ~ 현재 적용)
학술연구정보서비스(이하 RISS)는 정보주체의 자유와 권리 보호를 위해 「개인정보 보호법」 및 관계 법령이 정한 바를 준수하여, 적법하게 개인정보를 처리하고 안전하게 관리하고 있습니다. 이에 「개인정보 보호법」 제30조에 따라 정보주체에게 개인정보 처리에 관한 절차 및 기준을 안내하고, 이와 관련한 고충을 신속하고 원활하게 처리할 수 있도록 하기 위하여 다음과 같이 개인정보 처리방침을 수립·공개합니다.
주요 개인정보 처리 표시(라벨링)
목 차
3년
또는 회원탈퇴시까지5년
(「전자상거래 등에서의 소비자보호에 관한3년
(「전자상거래 등에서의 소비자보호에 관한2년
이상(개인정보보호위원회 : 개인정보의 안전성 확보조치 기준)개인정보파일의 명칭 | 운영근거 / 처리목적 | 개인정보파일에 기록되는 개인정보의 항목 | 보유기간 | |
---|---|---|---|---|
학술연구정보서비스 이용자 가입정보 파일 | 한국교육학술정보원법 | 필수 | ID, 비밀번호, 성명, 생년월일, 신분(직업구분), 이메일, 소속분야, 웹진메일 수신동의 여부 | 3년 또는 탈퇴시 |
선택 | 소속기관명, 소속도서관명, 학과/부서명, 학번/직원번호, 휴대전화, 주소 |
구분 | 담당자 | 연락처 |
---|---|---|
KERIS 개인정보 보호책임자 | 정보보호본부 김태우 | - 이메일 : lsy@keris.or.kr - 전화번호 : 053-714-0439 - 팩스번호 : 053-714-0195 |
KERIS 개인정보 보호담당자 | 개인정보보호부 이상엽 | |
RISS 개인정보 보호책임자 | 대학학술본부 장금연 | - 이메일 : giltizen@keris.or.kr - 전화번호 : 053-714-0149 - 팩스번호 : 053-714-0194 |
RISS 개인정보 보호담당자 | 학술진흥부 길원진 |
자동로그아웃 안내
닫기인증오류 안내
닫기귀하께서는 휴면계정 전환 후 1년동안 회원정보 수집 및 이용에 대한
재동의를 하지 않으신 관계로 개인정보가 삭제되었습니다.
(참조 : RISS 이용약관 및 개인정보처리방침)
신규회원으로 가입하여 이용 부탁 드리며, 추가 문의는 고객센터로 연락 바랍니다.
- 기존 아이디 재사용 불가
휴면계정 안내
RISS는 [표준개인정보 보호지침]에 따라 2년을 주기로 개인정보 수집·이용에 관하여 (재)동의를 받고 있으며, (재)동의를 하지 않을 경우, 휴면계정으로 전환됩니다.
(※ 휴면계정은 원문이용 및 복사/대출 서비스를 이용할 수 없습니다.)
휴면계정으로 전환된 후 1년간 회원정보 수집·이용에 대한 재동의를 하지 않을 경우, RISS에서 자동탈퇴 및 개인정보가 삭제처리 됩니다.
고객센터 1599-3122
ARS번호+1번(회원가입 및 정보수정)