The scrapping rate is increasing as various incentives are provided for the early scrapping of internal combustion engine vehicles and the purchase of electric vehicles. As a results, the amount of waste generated by end-of-life vehicles (ELVs) is increasing. Many countries, including Korea, are directing ELVs to comply with a recycling rate of 95% (including 10% of energy recovery). However, the recycling rate in Korea has not been reached since 2015, as about 89%. For these reasons, emphasizes the importance of improving recycling rate of ELVs.
To evaluate the recyclability and environmental properties of Automobile Shredder Residues (ASR) melting slag, characteristic analysis, leaching test and heavy metal analysis were conducted. The four types of bricks were manufactured using ASR melting slag; interlocking brick, clay brick, Asphalt paving aggregate, lightweight swelled ceramic brick. Density and absorption ratio of ASR slag were 2.24 g/㎤ and 0.34% respectively. The structure of slag from XRD analysis results were amorphous. Basicity (CaO/SiO<sub>2</sub>) was 1.01, this values are higher than general slag of municipal solid waste in Korea. The results of the leaching test, all of the pollutants measured in the satisfied the Korean standard. Heavy metals concentration in slag contained Fe, Al, Cr, Hg, and Cd very small amount relatively.
The interlocking brick substituted sand and stone powder by melting slag using as aggregates. As increasing melting slag content, absorption decreased and bending strength increased. Clay brick was manufactured for replacing kaolin and feldspar by melting slag that substituted by 20%. The quality of clay bricks mixed over 15% melting slag was not better than standard. Asphalt paving aggregate was investigating the optimum condition of slag content in mixed asphalt, the mixture ratio showed that 61% broken stone of 13 mm, 6% screenings, 10% melting slag, 15% sand and 8% of filler. A lightweight swelled ceramic brick was manufactured by using melting slag, front glass and so on. Specific gravity and compressive strength were ranged from 0.38 to 0.51 and from 339.7 to 373.6 N/㎠. The four types of bricks satisfied each KS quality and waste recycling standard.
This study, evaluated the possibility of material recycling using ASR. ASR was found to be effective not only for energy and material recovery, but also as a material recycling resource. Therefore, if the results of this study are applied for ASR recycling, it is expected that 95% of Korea ELVs recycling rate would be archived along with eco-friendly treatment.
분석정보
서지정보 내보내기(Export)
닫기소장기관 정보
닫기권호소장정보
닫기오류접수
닫기오류 접수 확인
닫기음성서비스 신청
닫기음성서비스 신청 확인
닫기이용약관
닫기학술연구정보서비스 이용약관 (2017년 1월 1일 ~ 현재 적용)
학술연구정보서비스(이하 RISS)는 정보주체의 자유와 권리 보호를 위해 「개인정보 보호법」 및 관계 법령이 정한 바를 준수하여, 적법하게 개인정보를 처리하고 안전하게 관리하고 있습니다. 이에 「개인정보 보호법」 제30조에 따라 정보주체에게 개인정보 처리에 관한 절차 및 기준을 안내하고, 이와 관련한 고충을 신속하고 원활하게 처리할 수 있도록 하기 위하여 다음과 같이 개인정보 처리방침을 수립·공개합니다.
주요 개인정보 처리 표시(라벨링)
목 차
3년
또는 회원탈퇴시까지5년
(「전자상거래 등에서의 소비자보호에 관한3년
(「전자상거래 등에서의 소비자보호에 관한2년
이상(개인정보보호위원회 : 개인정보의 안전성 확보조치 기준)개인정보파일의 명칭 | 운영근거 / 처리목적 | 개인정보파일에 기록되는 개인정보의 항목 | 보유기간 | |
---|---|---|---|---|
학술연구정보서비스 이용자 가입정보 파일 | 한국교육학술정보원법 | 필수 | ID, 비밀번호, 성명, 생년월일, 신분(직업구분), 이메일, 소속분야, 웹진메일 수신동의 여부 | 3년 또는 탈퇴시 |
선택 | 소속기관명, 소속도서관명, 학과/부서명, 학번/직원번호, 휴대전화, 주소 |
구분 | 담당자 | 연락처 |
---|---|---|
KERIS 개인정보 보호책임자 | 정보보호본부 김태우 | - 이메일 : lsy@keris.or.kr - 전화번호 : 053-714-0439 - 팩스번호 : 053-714-0195 |
KERIS 개인정보 보호담당자 | 개인정보보호부 이상엽 | |
RISS 개인정보 보호책임자 | 대학학술본부 장금연 | - 이메일 : giltizen@keris.or.kr - 전화번호 : 053-714-0149 - 팩스번호 : 053-714-0194 |
RISS 개인정보 보호담당자 | 학술진흥부 길원진 |
자동로그아웃 안내
닫기인증오류 안내
닫기귀하께서는 휴면계정 전환 후 1년동안 회원정보 수집 및 이용에 대한
재동의를 하지 않으신 관계로 개인정보가 삭제되었습니다.
(참조 : RISS 이용약관 및 개인정보처리방침)
신규회원으로 가입하여 이용 부탁 드리며, 추가 문의는 고객센터로 연락 바랍니다.
- 기존 아이디 재사용 불가
휴면계정 안내
RISS는 [표준개인정보 보호지침]에 따라 2년을 주기로 개인정보 수집·이용에 관하여 (재)동의를 받고 있으며, (재)동의를 하지 않을 경우, 휴면계정으로 전환됩니다.
(※ 휴면계정은 원문이용 및 복사/대출 서비스를 이용할 수 없습니다.)
휴면계정으로 전환된 후 1년간 회원정보 수집·이용에 대한 재동의를 하지 않을 경우, RISS에서 자동탈퇴 및 개인정보가 삭제처리 됩니다.
고객센터 1599-3122
ARS번호+1번(회원가입 및 정보수정)