Dental irreversible hydrocolloid impression materials are widely used in making dental casts for diagnosis, crown and bridge, partial dentures and complete dentures. It is important factor to make correct positive replica after impression taking, because most of prosthetics are produced indirectly with dental casts. The pH changes of irreversible hydrocolloid impression materials during gelation as the result of chemical reactions are directly associated with the setting of materials.
Some manufacturers use color agents that are pH dependent to indicate the stage of the material during setting, suggesting that the PH changes and the setting process of the material are linked each other.
The purpose of this study was to investigate the relationship between the pH change the occur during setting as chemical reactions develop among various components and the surface reproduction of dental stone.
Seven irreversible hydrocolloid impression materials (PAL, ALG, KRO, KAL, COE,
AXL and AXH) and dental gypsum products (Hi-K snf FUJ) were selected for the
experiment. The water-to-powder ratio was that recommended by the manufacturers of the materials. The overall experimental procedure was carried out in an environmental temperature of 21˚±1℃ and distilled water was used in mixing all materials. Each irreversible hydrocolloid specimen for pH measurements was placed in a plastic cylinder with an internal diameter of 30 mm and a height of 50mm. A small imprint was made on the surface of the gel to imprint the glass combined electrode of the pH meter (Microprocesssor pH/ion Meter DP-880 M, DMS, Korea) in the irreversible hydrocolloid mass. The surface of the imprint was covered with 0.5㎖ water to keep the pH meter electrode in continuous contact with the gel's aqueous phase. The pH change were recorded at 20 second intervals over a maximum period of 20 min, beginning 1 min after the start of mixing.
The surface reproduction was evaluated with steel test block described in A.D.A. specification 18 which has seven specified widths lines (0.025,0.050,0.075,0.1,0.15,0.2 and 0.3mm) and centered on the lines with the 0.20 mm cross line. The metal ring with an internal diameter of 30mm and a height of 20mm was placed on the steel test block and filled with irreversible hydrocolloid mass to overflowing. A flat clear glass was placed on top of each overfilled ring to eliminate the excess material. The test block and the
filled rings were placed tin a water bath, 10 min later removed and separated.
A new metal ring was placed on the irreversible hydrocolloid ring, and a gypsum
slurry was poured against the impression within 2 minutes. Thirty minutes later dental stone cast, sixty minutes later improved stone cast was removed. The quality of line reproduction was evaluated by visual observation under low-angle illumination from a microscope lamp.
From the experiment, the following results were obtained:
1. The irreversible hydrocolloid impression materials showed a significant difference in the pH changes from each other(p<0.01).
2. The pH values changed rapidly for the first 5 minutes from the start of mixing and then more slowly as setting occurred before they progressively stabilized toward the end of the 20 minutes period.
3. The surface reproduction of irreversible hydrocolloid impression materials was superior in acidic and closer to the neutral pH values(p<0.01).
4. There is no significant difference of surface reproduction between the dental stone and improved stone(p<0.01).
서지정보 내보내기(Export)
닫기소장기관 정보
닫기권호소장정보
닫기오류접수
닫기오류 접수 확인
닫기음성서비스 신청
닫기음성서비스 신청 확인
닫기이용약관
닫기학술연구정보서비스 이용약관 (2017년 1월 1일 ~ 현재 적용)
학술연구정보서비스(이하 RISS)는 정보주체의 자유와 권리 보호를 위해 「개인정보 보호법」 및 관계 법령이 정한 바를 준수하여, 적법하게 개인정보를 처리하고 안전하게 관리하고 있습니다. 이에 「개인정보 보호법」 제30조에 따라 정보주체에게 개인정보 처리에 관한 절차 및 기준을 안내하고, 이와 관련한 고충을 신속하고 원활하게 처리할 수 있도록 하기 위하여 다음과 같이 개인정보 처리방침을 수립·공개합니다.
주요 개인정보 처리 표시(라벨링)
목 차
3년
또는 회원탈퇴시까지5년
(「전자상거래 등에서의 소비자보호에 관한3년
(「전자상거래 등에서의 소비자보호에 관한2년
이상(개인정보보호위원회 : 개인정보의 안전성 확보조치 기준)개인정보파일의 명칭 | 운영근거 / 처리목적 | 개인정보파일에 기록되는 개인정보의 항목 | 보유기간 | |
---|---|---|---|---|
학술연구정보서비스 이용자 가입정보 파일 | 한국교육학술정보원법 | 필수 | ID, 비밀번호, 성명, 생년월일, 신분(직업구분), 이메일, 소속분야, 웹진메일 수신동의 여부 | 3년 또는 탈퇴시 |
선택 | 소속기관명, 소속도서관명, 학과/부서명, 학번/직원번호, 휴대전화, 주소 |
구분 | 담당자 | 연락처 |
---|---|---|
KERIS 개인정보 보호책임자 | 정보보호본부 김태우 | - 이메일 : lsy@keris.or.kr - 전화번호 : 053-714-0439 - 팩스번호 : 053-714-0195 |
KERIS 개인정보 보호담당자 | 개인정보보호부 이상엽 | |
RISS 개인정보 보호책임자 | 대학학술본부 장금연 | - 이메일 : giltizen@keris.or.kr - 전화번호 : 053-714-0149 - 팩스번호 : 053-714-0194 |
RISS 개인정보 보호담당자 | 학술진흥부 길원진 |
자동로그아웃 안내
닫기인증오류 안내
닫기귀하께서는 휴면계정 전환 후 1년동안 회원정보 수집 및 이용에 대한
재동의를 하지 않으신 관계로 개인정보가 삭제되었습니다.
(참조 : RISS 이용약관 및 개인정보처리방침)
신규회원으로 가입하여 이용 부탁 드리며, 추가 문의는 고객센터로 연락 바랍니다.
- 기존 아이디 재사용 불가
휴면계정 안내
RISS는 [표준개인정보 보호지침]에 따라 2년을 주기로 개인정보 수집·이용에 관하여 (재)동의를 받고 있으며, (재)동의를 하지 않을 경우, 휴면계정으로 전환됩니다.
(※ 휴면계정은 원문이용 및 복사/대출 서비스를 이용할 수 없습니다.)
휴면계정으로 전환된 후 1년간 회원정보 수집·이용에 대한 재동의를 하지 않을 경우, RISS에서 자동탈퇴 및 개인정보가 삭제처리 됩니다.
고객센터 1599-3122
ARS번호+1번(회원가입 및 정보수정)