KCI등재
티타늄과 금합금, 은-팔라듐합금 및 니켈-크롬 합금의 접촉시 부식에 관한 연구 = CORROSION STUDIES ON TITANIUM IN CONTACT WITH GOLD, SILVER-PALLADIUM AND NICKEL-CHROMIUM ALLOYS IN VITRO
저자
김춘호 (조선대학교 치과대학 보철학교실) ; 고영무 (조선대학교 치과대학 치과재료학교실) ; 계기성 (조선대학교 치과대학 보철학교실)
발행기관
학술지명
대한치과재료학회지(THE JOURNAL OF THE KOREA RESEARCH SOCIETY FOR DENTAL MATREIALS)
권호사항
발행연도
1994
작성언어
Korean
KDC
515.12
등재정보
KCI등재
자료형태
학술저널
발행기관 URL
수록면
37-58(22쪽)
제공처
소장기관
The Purpose of this study was to evaluate the effect of area ratio, the difference of the corrosion rate according to the elapsed time, and corrosion reaction on titanium in contact with gold alloy, silver-palladium alloy, and nickel-chromium alloy by measuring the amount of metal elements released in the artificial saliva using Inductively Coupled Plasma Emission Spectroscopy(ICPES).
The specimen of 15 titanium plates, 5 gold alloy plates, 5 silver-palladium alloy plates, 5 nickel-chromium alloy plates and 20 acrylic resin plates were fabricated, and also the specimen of 60 titanium plugs, 30 gold alloy plugs, 30 silver-palladium alloy plugs and 30 nickel-chromium alloy plugs were fabricated.
The amount of metal elements released when titanium, gold alloy, silver-palladium alloy and nickel-chromium alloy immersed solely in the artificial saliva solution of 70ml, and the galvanic corrosion reaction occurred on the titanium in contact with gold alloy, silver-palladium alloy, and nickel-chromium alloy were observed during 21 weeks in the interval of each 7 week using immersion test, and then the amount of metal elements released in the artificial saliva solution was measured using ICPES.
From the experiments, the following results were obtained :
1. In case of immersing titanium, gold alloy, silver-palladium alloy, and nickel-chromium alloy solely in the artificial saliva solution (Group 1, 2, 3, and 4), the total amount of metal elements released was that group 4 was greater about 2.3 times than group 3, and about 7.8 times than group 2. In case of group 1, the amount of titanium released was not found after 8 week(p<0.001)
2. In case of galvanic coupling of titanium in contact with gold alloy(Group 5, 6), the total amount of metal elements released of group 5 and 6 was less than that of group 7, 8, 9, and 10(p<0.05).
3. In case of galvanic coupling of titanium in contact with silver-palladium alloy(Group 7, 8), the total amount of metal elements released of group 7 was greater about twice than that of group 5, and that of group 8 was about 14 times than that of group 6(p<0.05).
4. In case of galvanic coupling of titanium in contact with nickel-chromium alloy(Group 9, 10), the total amount of metal elements released of group 9 and 10 was greater about 1.8∼3.2 times than that of group 7 and 8, and was greater about 4.3∼25 times than that of group 5,6(p<0.05).
5. In the effect of galvanic corrosion according to the difference of the area ratio of cathode and anode, the total amount of metal elements released was that group 5 was greater about 4 times than group 6, group 8 was greater about twice than group 7, and group 10 was greater about 1.5 times than group 9(p<0.05).
6. In the effect of galvanic corrosion according to the elasped time during 21 weeks in the interval of each 7 week, the amount of metal elements released was decreased markedly in case of galvanic coupling of the titanium in contact with gold alloy and silver-palladium alloy but the total amount of nickel and beryllium released was not decreased markedly in case of galvanic coupling of the titanium in contact with nickel-chromium alloy(p<0.05)
In conclusion, not only in case of immersing nickel-chromium alloy solely in the artificial saliva solution(Group 4) but also in case of galvanic coupling of the titanium in contact with nickel-chromium alloy(Group 9, 10), the total amount of metal elements released of group 4, 9 and 10 was greater than that of group 5, 6, 7 and 8, and there was greater about 4.3∼25 times than that of group 5 and 6, and therefore, it was considered that the corrosion behavior of nickel-chromium alloy had more problem than that of gold alloy and silver-palladium and futher research is needed.
서지정보 내보내기(Export)
닫기소장기관 정보
닫기권호소장정보
닫기오류접수
닫기오류 접수 확인
닫기음성서비스 신청
닫기음성서비스 신청 확인
닫기이용약관
닫기학술연구정보서비스 이용약관 (2017년 1월 1일 ~ 현재 적용)
학술연구정보서비스(이하 RISS)는 정보주체의 자유와 권리 보호를 위해 「개인정보 보호법」 및 관계 법령이 정한 바를 준수하여, 적법하게 개인정보를 처리하고 안전하게 관리하고 있습니다. 이에 「개인정보 보호법」 제30조에 따라 정보주체에게 개인정보 처리에 관한 절차 및 기준을 안내하고, 이와 관련한 고충을 신속하고 원활하게 처리할 수 있도록 하기 위하여 다음과 같이 개인정보 처리방침을 수립·공개합니다.
주요 개인정보 처리 표시(라벨링)
목 차
3년
또는 회원탈퇴시까지5년
(「전자상거래 등에서의 소비자보호에 관한3년
(「전자상거래 등에서의 소비자보호에 관한2년
이상(개인정보보호위원회 : 개인정보의 안전성 확보조치 기준)개인정보파일의 명칭 | 운영근거 / 처리목적 | 개인정보파일에 기록되는 개인정보의 항목 | 보유기간 | |
---|---|---|---|---|
학술연구정보서비스 이용자 가입정보 파일 | 한국교육학술정보원법 | 필수 | ID, 비밀번호, 성명, 생년월일, 신분(직업구분), 이메일, 소속분야, 웹진메일 수신동의 여부 | 3년 또는 탈퇴시 |
선택 | 소속기관명, 소속도서관명, 학과/부서명, 학번/직원번호, 휴대전화, 주소 |
구분 | 담당자 | 연락처 |
---|---|---|
KERIS 개인정보 보호책임자 | 정보보호본부 김태우 | - 이메일 : lsy@keris.or.kr - 전화번호 : 053-714-0439 - 팩스번호 : 053-714-0195 |
KERIS 개인정보 보호담당자 | 개인정보보호부 이상엽 | |
RISS 개인정보 보호책임자 | 대학학술본부 장금연 | - 이메일 : giltizen@keris.or.kr - 전화번호 : 053-714-0149 - 팩스번호 : 053-714-0194 |
RISS 개인정보 보호담당자 | 학술진흥부 길원진 |
자동로그아웃 안내
닫기인증오류 안내
닫기귀하께서는 휴면계정 전환 후 1년동안 회원정보 수집 및 이용에 대한
재동의를 하지 않으신 관계로 개인정보가 삭제되었습니다.
(참조 : RISS 이용약관 및 개인정보처리방침)
신규회원으로 가입하여 이용 부탁 드리며, 추가 문의는 고객센터로 연락 바랍니다.
- 기존 아이디 재사용 불가
휴면계정 안내
RISS는 [표준개인정보 보호지침]에 따라 2년을 주기로 개인정보 수집·이용에 관하여 (재)동의를 받고 있으며, (재)동의를 하지 않을 경우, 휴면계정으로 전환됩니다.
(※ 휴면계정은 원문이용 및 복사/대출 서비스를 이용할 수 없습니다.)
휴면계정으로 전환된 후 1년간 회원정보 수집·이용에 대한 재동의를 하지 않을 경우, RISS에서 자동탈퇴 및 개인정보가 삭제처리 됩니다.
고객센터 1599-3122
ARS번호+1번(회원가입 및 정보수정)